THE MAKING OF MATCHES

11%

Seventh-day Adventist Publishing Association · Battle Creek, Mich. · Mar 15, 1898

FromReview and Herald, Vol. 75, No. 11.

Read the full edition

THE MAKING OF MATCHES.

From the days of flint, steel, and tinder to the present, the development in the means of producing an artificial light or kindling a fire has been commensurate with that in other departments of life, and has far removed the tedious methods and devices of a few decades ago from even the knowledge of the present active generation.
Nearly every one is familiar with the pink-headed English matches, and this is how they are made: The timber from which the splints are made is in the form of twenty-foot logs of whitewood, imported from Russia. In dealing with the timber, which must be properly selected and prepared, the first step is to saw the logs into lengths of two or three feet, which are then conveyed to the match department or to the box-making room.
The matches are made from a strip of veneer, or a sheet of wood the thickness of the match. This veneer is produced from the round log placed in a peeling-machine, which is an ingeniously contrived arrangement somewhat on the principle of a lathe, but the wood is turned off into one endless strip, in width corresponding to the length of the log. A number of strips thus cut are placed one upon the other, and passed through a cutting-machine, which acts on the guillotine principle, and chops the strips into thousands of splints, each the exact length and shape required for a single match.
One machine is capable of producing about twelve million splints an hour. They fall from the blade in a torrent, each being cleanly divided from the other, and free from irregularities in shape. They are then thoroughly dried in a special form of apparatus by means of which enormous quantities can be treated in the course of a few hours. This machine can, if necessary, be kept constantly at work, and is a decided improvement upon the ordinary methods adopted for splint-drying.
When thoroughly dried, the splints, still in an indiscriminate heap, no two being in the same position, must be arranged side by side. This is done by machines which shake the splints about in such a way that they drop into compact rows, each splint parallel with all the others. While this is being done, they are freed from dust and loose particles of wood.
From these machines the splints are taken to be placed in frames. Each frame measures about three feet square, and is fitted with a number of bars, crossing one another, between which the splints are held, each splint occupying a separate place. This is also done by mechanism, which enables about four thousand splints to be deftly fitted into a frame in less than a minute.
The frames, thus filled with splints, are wheeled away on trolleys to the paraffining-room, where the end which is to receive the head is first heated and then dipped into paraffin. Then they are taken to the composition-stones, of which there is a long row, each covered with a bright-pink semi-liquid preparation. At each stone stands a workman, who lifts the frames, one after the other, and dips the ends of the splints into the chemical composition, taking care that they are all well supplied with a full, round, firm head.
The frames are then again placed upon trolleys and taken to the drying-rooms, each of which is capable of drying about a thousand gross a day. The matches, when free from moisture, are ready to be put into the boxes of various shapes and sizes in which they reach the consumer.—Selected.