In the so-called “greenhouses” a large quantity of ware is drying, preparatory to being “fired.” This process is the crucial test of pottery. All the preceding operations have been carefully conducted with a distant view to this one. All the combinations of clay, flint, stone, or bone have been made with forethought of the kiln in which the ware will be partially vitrified. Earthenware and porcelain are only, as it is well known, less perfect forms of glass, or rather of glass in another stage of development. When the earthenware slip cups and saucers, mugs and jugs, are sufficiently dried, they are ready for the “biscuit” kilns, as they are oddly called, for the ware is not twice baked in them, nor is it good to eat. Some kinds of ware are submitted to the intense heat of the kiln three times, all twice—once in biscuit and once in glaze. When painting is introduced over the glaze, as in the old Sevres pate tendre and the various kinds of fine porcelain, there is a third firing. Before being placed in the kilns, all the articles thrown, turned, or molded are arranged in “seggars,” receptacles of coarse clay, very thick and strong, like deep pie dishes. Into these the various articles are packed with considerable skill, little triangles being placed between each to prevent their touching each other, and the seggars are next packed together in the kiln or oven, each seggar being lined at the bottom with a layer of rock sand. Piled one on the other, the seggars make a fairly compact column, and when the oven, some nineteen feet in altitude, is filled, the fire is applied. It will be understood that the fire by no means touches either the ware or the seggars in which it is enclosed. They are simply in an oven about to be raised to a tremendous heat. The firing is done by means of flues so arranged as to diffuse intense heat throughout the whole interior of the ovens. This firing is a ticklish operation, requiring the supervision of a skilled workman capable of going without sleep for some thirty-six or forty hours. At first the heat is applied gently for fear of cracking the ware, and the fireman has an anxious time of it. Little openings in the brickwork enable him to judge of the progress of his work. The heat of the biscuit oven during the last twenty-four hours is intense. As the ware has taken from forty to fifty hours in firing, so does it require an equal time to become cool.—The Interior.
HOW CUPS AND SAUCERS ARE MADE.
From The Youth’s Instructor, Vol. 33, No. 48., December 16, 1885