AdventAI

Wood fibers capable of being spun are now prepared in Germany. The process is as follows: Boards as free from knots as possible, of any desired width, and about three-eighths of an inch thick, are cut in a direction parallel with the fiber, preferably from pine or fir wood or from the softer part of larch, and are boiled in a solution of sulphurous acid or a bisulphite, whereby the disintegration of the wood is effected. No chopping is required, and before boiling, the wood is steamed at 212° Fahr. for a long time. After boiling, the mass is partly dried on a wooden frame, and then passed through rollers having “deep ribs” in the direction of their length, the projections on one roller fitting in the corrugations of the other, whereby the fibers will be separated from each other, and may be combed in an apparatus similar to that for combing flax, etc.