THE PROCESS OF GOLD-BEATING

13%

S. D. A. Publishing Association · Battle Creek, Mich. · Dec 5, 1895

FromThe Youth’s Instructor, Vol. 43, No. 49.

Read the full edition

THE PROCESS OF GOLD-BEATING.

The following facts relating to the art of gold-beating are taken from the Argosy:—
“The gold to be used is alloyed with silver or copper, according to the color desired, and cast in ingots four inches in length, and weighing from ten to seventeen ounces. The second process consists in passing the four-inch ingot between polished steam rollers. This reduces the gold to a ribbon twenty-eight yards in length, and one eight-hundredth part of an inch in thickness. Seven yards of this ribbon are cut into one hundred and eighty pieces one inch square. These are placed singly between the leaves of a bundle of vellum, technically known as a ‘cutch.’
“They are then inclosed in a parchment case, and beaten for half an hour with a twenty-pound hammer. By this time the gold is extended into squares of three inches. These are removed from the cutch, and quartered.
“The next tool used is called a ‘showder.’ It consists of seven hundred and twenty ‘gold beaters’ skins’ four inches square. The gold beaters’ skins are bought in packets of nine hundred leaves, and for each packet the intestines of five hundred oxen are required. They are manufactured from the outer membrane of the large intestine by an exceedingly offensive process, as the intestine requires to be subjected to partial putrefaction before it can be separated from the membrane.
“Although the skins have a delicate appearance and are beaten for several hours every day with a ten-pound hammer, they generally last about a year, when they are renewed for thirty-five or forty dollars. The seven hundred and twenty pieces of gold are beaten in the showder for an hour and a quarter, till they increase from one and a half to four inches square.
“Another quartering then takes place, and the pieces are then placed between the skins in a tool called a ‘mold,’ and beaten for a third time. This mold is filled three times, thus producing two thousand eight hundred and eighty leaves from the eighty pieces. It has been beaten altogether about five hours. The cutch, the showder, and the mold, before being filled with gold, are subjected to treatment in hot presses, formed on the principle of a letter-press, for the purpose of clearing the tools from damp.
“With an instrument called a ‘wagon’ the gold is cut to its final size (a square of three and three-eighths inches), and is then lifted into books of tissue paper, the leaves of which have been previously rubbed with red chalk to prevent adhesion. The leaf is now only one two-hundred-and-eighty thousandth of an inch in thickness, and when held up to the light appears to be green. It is calculated that one ounce of gold may be converted into leaf sufficient to gild silver wire about thirteen hundred miles in length.”